Shear bond strength between gingival composite resin and glazed gingival porcelain for implant-supported prostheses

Futoshi Komine, Kei Kubochi, Fumiaki Kimura, Kosuke Kusaba, Ryoki Takano, Hideo Matsumura

研究成果: ジャーナルへの寄稿記事査読

1 被引用数 (Scopus)

抄録

This study determined the shear bond strength (SBS) between an indirect gingival composite resin and glazed gingival porcelain after various surface treatments. A total of 176 porcelain disks with natural glazing were used and assigned to one of four groups: no surface treatment, airborne-particle abrasion, hydrofluoric acid etching, or a combination of airborne-particle abrasion followed by hydrofluoric acid etching. Each group was divided into two subgroups: one subgroup was unprimed, and the other was silanized. An indirect composite resin was then bonded to the porcelain disks. Half of the specimens in each group (n = 11) were exposed to 5000 thermocycles. SBSs were measured, and data were analyzed with the Kruskal–Wallis and Steel–Dwass tests. Among silanized specimens, those treated with the combination of airborne-particle abrasion and hydrofluoric acid etching exhibited the highest bond strengths both before and after thermocycling. However, the SBS values of the silanized and unprimed hydrofluoric acid etched specimens did not differ significantly. Airborne-particle abrasion followed by hydrofluoric acid etching with silane application yielded stronger, more durable bonds between the indirect gingival composite resin and glazed gingival porcelain.

本文言語英語
論文番号e12762
ジャーナルEuropean Journal of Oral Sciences
129
2
DOI
出版ステータス出版済み - 4月 2021

フィンガープリント

「Shear bond strength between gingival composite resin and glazed gingival porcelain for implant-supported prostheses」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル