抄録
Although there have been improvements in bracket systems precoated with adhesive, removal of adhesive remnants continues to be problematic. This study compared the hardness and maintainability of precoated adhesive with other commercial adhesives. Knoop hardness values were measured after light-or chemical-induced initial curing, immersion in distilled water at 37°C for 24 h and 1,000 and 10,000 thermal cycles after 24 h. Additionally, the forces required to move brackets by 0.5 mm were measured during bracket positioning, and brackets bonded to bovine enamel were examined by field-emission scanning electron microscopy. The Knoop hardness values of the precoated adhesives were lower than those of commercial resin composite adhesives, and hardness was dependent on the amount of filler in the resin matrix. The ability to maintain the device position may depend on the resin matrix composition. Precoated adhesives with less filler and more matrix material are light curable, and remnant resin may be easily removed.
本文言語 | 英語 |
---|---|
ページ(範囲) | 48-51 |
ページ数 | 4 |
ジャーナル | Journal of Oral Science |
巻 | 62 |
号 | 1 |
DOI | |
出版ステータス | 出版済み - 1月 2020 |