We obtained amorphous-FeAs-free SmFeAsO1-xFx using a low temperature sintering with slow cooling. SmFeAsO1-xFx is sintered at 980 °C for 40h and cooled slowly down to 600 °C. The low temperature sintering suppresses the formation of amorphous FeAs, and the slow cooling introduces much fluorine into SmFeAsO1-xFx. The superconductivity of this sample appears at 57.8 K and the superconducting volume fraction reaches 96%. To study the change of fluorine concentration during the cooling process, samples are quenched by water at 950, 900, 850, 800, 750, and 700 °C. It is found that fluorine is substituted not only at the maximum heating temperature but also during the cooling process. The low temperature sintering with slow cooling is very effective to obtain a homogeneous SmFeAsO1-xFx with high fluorine concentration.

本文言語英語
論文番号094707
ジャーナルJournal of the Physical Society of Japan
82
9
DOI
出版ステータス出版済み - 9月 2013
外部発表はい

フィンガープリント

「α-feas-free SmFeAsO1-xFx by low temperature sintering with slow cooling」の研究トピックを掘り下げます。これらがまとまってユニークなフィンガープリントを構成します。

引用スタイル